[mems-talk] Silicon resistivity for comb-actuation
bob hou
managerbcm02 at yahoo.com
Sun Mar 23 01:55:56 EST 2008
I think it is better to observe the movement by Wyko/Zyko, which apply the interference principle and is sensitive to see the tiny movement.
BR
my2232 at columbia.edu wrote:
Hello all,
I am trying to actuate a comb-actuator. However, I was not able to see
any movement under Karl Suss probe station.
The resistivity of my SOI wafer is 1-30 Ohmcm. Dopant tytpe is P/Boron.
The wafer is from ULTRASIL.
I am applying a static voltage differenece, i am not interested about
dynamic voltages for now. Is it a problem to use 1-30 Ohmcm
resistivity Silicon.
Thanks in advance,
Mehmet Yilmaz
PhD student
Mechanical engineer
More information about the MEMS-talk
mailing list