Spitting is caused by hot spots. I would recommend a lower deposition
rate or a much slower ramp-up process.
Dan
-----Original Message-----
From: mems-talk-bounces at memsnet.org
[mailto:mems-talk-bounces at memsnet.org] On Behalf Of Daniel Fine
Sent: Monday, March 31, 2008 8:08 AM
To: mems-talk at memsnet.org
Subject: [mems-talk] Pyrex ebeam evaporation
Hello,
My name is Daniel Fine and I am a post doc at the University of Texas
at Austin. I am trying to ebeam evaporate Pyrex (7740) and am running
into a problem where I am finding it hard to prevent bubbling and thus
spitting of the material when I try to achieve deposition rates of 5
Angstrom per second or higher. The films are therefore covered with
non-uniform streaks of Pyrex. I am using a CHA evaporator. I have
tried a steady beam spot in one place and an oscillating beam spot as
well but get the same problem of large bubble formation. I would
greatly appreciate any input concerning how I might over come this
problem.
Thanks,
Daniel Fine