[mems-talk] Gold evaporation coating on silicon.

Andrea Mazzolari mazzolari at fe.infn.it
Thu May 1 11:04:32 EDT 2008


Hello,
i whould suggest you to deposit some nm of cr before gold deposition.
Best regards,
Andrea

> Hello
>
> I want to coat silicon with evaporation coating, and
> to assurance that the adhesion between the two
> materials  will be optimal.
> What will be  the optimal treatment to achieve
> adhesion ?