[mems-talk] Gold evaporation coating on silicon
Michael Larsson
michael.larsson at gmail.com
Thu May 1 14:03:21 EDT 2008
Hi Moshe,
What material are you trying to get to adhere to the Si surface, and
what is the application? Au is suitable for some applications because
it provides a clean, oxide-free surface that can improve chemical
adhesion with some materials.
Michael
> ---------- Forwarded message ----------
> From: Moshe <moduli0621 at yahoo.com>
> To: mems-talk at memsnet.org
> Date: Wed, 30 Apr 2008 22:14:14 -0700 (PDT)
> Subject: [mems-talk] Gold evaporation coating on silicon.
> Hello
>
> I want to coat silicon with evaporation coating, and
> to assurance that the adhesion between the two
> materials will be optimal.
> What will be the optimal treatment to achieve
> adhesion ?
More information about the MEMS-talk