Hi All,

Does anyone know of a wet chemical etch for 316L stainless steel? We're
trying to uniformly etch away, or at least thin, 100um of stainless steel
from a magnesium diboride core. It would be nice if the magnesium diboride
core was not etched, or at least etched at a much slower rate than the
stainless steel.