[mems-talk] metal on tungsten

Richard B. Keithley rbk at email.unc.edu
Sun May 11 16:42:49 EDT 2008


 From my personal experience I know gold and platinum work well.  We 
have a paper in Langmuir that uses Tungsten microwires as a substrate 
and electrodeposits gold and platinum.  The paper was for wires so if 
you want to deposit on a chip, you may have to adapt the procedure a 
bit.

Conical Tungsten Tips as Substrates for the Preparation of 
Ultramicroelectrodes.  Langmuir, 22 (25), 10348 -10353, 2006.

Best,

-Richard

Richard B. Keithley
UNC Analytical Chemistry Graduate Student &
National Defense Science and Engineering Graduate Fellow
Wightman Research Group
Chapel Hill, NC 27599
919-962-1108

Quoting Andrea Mazzolari <mazzolari at fe.infn.it>:

> Hi all,
>
> i need to deposit about 20um of any metal on tungsten.
> Could someone suggest a metal which have good adhesion to tungsten and an
> appropriate deposition technique ?
>
> For my understanding Titanium deposited by electrodeposition should work
> fine, but i don't have a big experience.


More information about the MEMS-talk mailing list