[mems-talk] Solvent effects on Teflon AF

Brubaker Chad C.Brubaker at EVGroup.com
Mon May 12 14:01:24 EDT 2008


Teimour,

Teflon AF should not actually be soluble in IPA. However, depending on
method of use, it may cause mechanical removal (peelng).


Best Regards,
Chad Brubaker

EV Group 
invent * innovate * implement
Senior Process Technology Engineer - Direct: +1 (480) 305 2414, Main: +1
(480) 305 2400 Fax: +1 (480) 305 2401
Cell: +1 (602) 321 6071
E-Mail: C.Brubaker at EVGroup.com, Web: www.EVGroup.com
 
-----Original Message-----
From: mems-talk-bounces at memsnet.org
[mailto:mems-talk-bounces at memsnet.org] On Behalf Of Teimour Maleki
Sent: Friday, May 09, 2008 8:07 AM
To: 'General MEMS discussion'
Subject: [mems-talk] Solvent effects on Teflon AF

Dear all,

 Does anybody know what is the effect of IPA on Teflon AF coated
substrate?
When I used IPA, it will remove the Teflon.