[mems-talk] PDMS glue recommandation

Teimour Maleki t.maleki at gmail.com
Wed May 28 13:01:09 EDT 2008


What do you want to attach together? I used crazy glue from walmart, it
works fine for tubing!!
Have fun,
 

-----Original Message-----
From: mems-talk-bounces at memsnet.org [mailto:mems-talk-bounces at memsnet.org]
On Behalf Of Hong Chen
Sent: Wednesday, May 28, 2008 11:37 AM
To: mems-talk at memsnet.org
Subject: [mems-talk] PDMS glue recommandation

Hi,

is there anyone can recommend a PDMS glue? I found epoxy-based and
ethylene- vinyl- acetate-based is not useful. Well, you can use PDMS
as the glue but the problem is it trends to spread and occupy every
spaces it can reach including your micro channels.