Hello all,

One of my work colleagues maintains it is possible to anodically bond 
III-V semiconductors (specifically GaAs) to both silicon and silicon 
nitride. Even when I explained to him that the anodic bonding process 
relies on the presence of metal alkaki oxides (e.g. NaO) he still stood 
by his claim!

Has anyone anodically bonded a III-V material?

If I wanted to permanently bond GaAs to a thin SiN layer what technique 
should I use? Thermocompression, Fusion?