Hi all,
I am searching for a photoresist that is sensitive to visible wavelength of
light.
especially in 600-800 nm region. I found a conference paper in which SU-8
3050BW.
a photoresist sensitive to visible range of light, was used. However, I
could not find any information about SU-8 3050BW.
Or is it possible to modify conventional photoresist to be sensitive to
visible spectrum by using photoinitiator and photosensitizer?