If you have CR-7 (Cr etchant) around, we measured an Ag etch rate of 450 nm/min in it. --Kirt Williams, Ph.D., consultant ----- Original Message ----- From: Helen LiTo: Sent: Monday, April 21, 2003 11:24 AM Subject: [mems-talk] wet-etching of silver > Hi, > > Can anyone tell me the recipe for wet-etching of > silver film (on glass substrate)? > > Thanks so much, > Helen > > > __________________________________________________ > Do you Yahoo!? > The New Yahoo! Search - Faster. Easier. Bingo > http://search.yahoo.com > > _______________________________________________ > MEMS-talk@memsnet.org mailing list: to unsubscribe or change your list > options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk > Hosted by the MEMS Exchange, providers of MEMS processing services. > Visit us at http://www.memsnet.org/