Hi,
Is there anyone know which etchant is the best one for anisotropic Cu
wet etching or any similar way in good control of Cu good sidewall
definition in terms of wet etching? How to control the etch rate?

I am using Al etchant, but it does not works very well.

Thanks.

Johnny