Transene makes one called TFA that is pretty good. It takes less than 20 seconds for it to etch 1000A of Au, and I had no problems with it. Jesse Fowler UCLA/MAE Dept., 420 Westwood Plaza, Room 37-129, ENGR IV Los Angeles, CA 90095-1597 | (310)825-3977 "Observations of nature, no matter how seemingly arcane, are like peeling off one more layer from the great onion of knowledge" -- Don Petit, ISS science officer On Wed, 30 Apr 2003, Sang Hwui Lee wrote: > Hello, > > Does anyone know the recipe of Au etchant or the product name for Au > etchant? I have Au/Cr deposited pyrex glass wafer. now I don't have Au > etchant. Au etchant should not attack Cr layer or interface of Cr/glass > since Au/Cr would be window for glass isotropic etching in BOE. > > thanks, > > SangHwui Lee > Ph.D candidate/MSE/NJIT > Microelectronics Research Center(MRC) > 973-596-6368(O) > 201-242-1486(H) > > > > > > _________________________________________________________________ > MSN 8 helps eliminate e-mail viruses. Get 2 months FREE*. > http://join.msn.com/?page=features/virus > > > _______________________________________________ > MEMS-talk@memsnet.org mailing list: to unsubscribe or change your list > options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk > Hosted by the MEMS Exchange, providers of MEMS processing services. > Visit us at http://www.memsnet.org/ >