We can provide alumina etching services on silicon / glass wafers. What thickness is your alumina? Gautham Viswanadam; Managing Director, Absara Micro Systems (S) Pte Ltd; 17, Philips Street, #05 - 01; Grand Building Singapore - 048695. Ph: 65 64841430 Fax: 65 64842780; e-mail: absara@singnet.com.sg ----- Original Message ----- From: "Louis Chomas"To: Sent: Wednesday, May 07, 2003 12:05 AM Subject: [mems-talk] Alumina Etchants > I'm trying to etch some alumina films and was wondering if anyone > had any suggestions for etchants or thoughts on where I could look to > get some information/data on etching alumina. > > Thanks, > Lou Chomas > > > _______________________________________________ > MEMS-talk@memsnet.org mailing list: to unsubscribe or change your list > options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk > Hosted by the MEMS Exchange, providers of MEMS processing services. > Visit us at http://www.memsnet.org/