Cr and Au deposition by using sputter
2003-05-07
2003-05-07
R. Brent Garber (2 parts)
2003-05-07
2003-05-08
Cr and Au deposition by using sputter
BobHendu@aol.com
2003-05-07
You probably have a leak in your sputtering system. If deposited properly chrome
layer should not be green. Bob Henderson