Amit, MEMSCAP acquired the group that was formerly Cronos from JDS Uniphase. We still run the original MUMPS process. We also run two new MUMPS processes, SOI MUMPS and Metal MUMPS, along with the original Poly MUMPS. You can access the design rules and place orders on the website: http://www.memsrus.com/CIMSsvcs.html If you have any questions, feel free to contact Buzz Hardy at (919)314-2235. -Mark Stonefield -----Original Message----- From: Amit Savkar [mailto:asavkar@engr.uconn.edu] Sent: Wednesday, May 07, 2003 6:57 PM To: mems-talk@memsnet.org Subject: [mems-talk] Fabrication of MEMS Device Dear All, This is Amit Savkar a Phd Candidate at University of Connecticut at Storrs. I am a new member to this discussion group, and would like to ask a few basic questions regarding fabrication of MEMS device. Our research group is actively seeking vendors who can actually fabricate a device, with decent reliability. We have particulars of this device and would like to know vendors, universities who had reliable established MUMPS process for fabrication. It would be highly appreciated if any fellow members can throw light on the same. Thanks Regards Amit Savkar PhD Candidate University of Connecticut Department of Mechanical Engineering Dynamics and Vibration Lab 191 Auditorium Road U 3139 Storrs CT 06226 Lab : 860 486 5339