durusmail: mems-talk: PMMA protection during TMAH etching
PMMA protection during TMAH etching
PMMA protection during TMAH etching
Sreemanth M Venkata Uppuluri
2003-05-12
Hi Yilel

PMMA doesn't dissolve in TMAH. So you do not need any protective coating
to cover it.

regards
Sreemanth

On Sat, 10 May 2003, Yilei Zhang wrote:

> Hello members:
> May anyone tell me how to protect PMMA coating during TMAH etching? Is PMMA
> soluble in TMAH? Thanks.
>
> Regards,
> Yilei Zhang
>
>
>
>
> _______________________________________________
> MEMS-talk@memsnet.org mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/
>