Hello everyone,

Does anybody have an experience with Aluminium etching for several hundred nm-
pitch gratings?
I am using BCl3, Cl2, O2 gases for the etching.  But, PR damage is severe.
Could you tell me proper etch mask, gas ratios, rf power, etc?
Thank you in advance.

Sincerely,
Seh-Won Ahn