you may want to check http://www.micromachines.com/, they have good prices ($20,$50) for bow, stress measurements. Good Luck _________________________ Erhan Ata NanoDevices, Inc. erhan@nanodevices.com Tel :805-696-9002 ext.203 Fax:805-696-9003 -----Original Message----- From: Robert D White [mailto:rdwhite@engin.umich.edu] Sent: Wednesday, May 21, 2003 7:14 AM To: mems-talk@memsnet.org Subject: [mems-talk] Wafer Curvature Measurements I am looking for someone to do some pre- and post- wafer curvature measurements for estimation of residual stresses evolved during LPCVD deposition. I would be doing the LPCVD step myself, and want to send the wafers somewhere to get the measurements done before and after. Does anyone offer this service or know where I might look? Many thanks, Rob -- Robert D. White Graduate Student Research Assistant Vibrations and Acoustics Lab, 2200 EECS Mechanical Engineering University of Michigan Ann Arbor, MI 48109 (734)936-3824 rdwhite@umich.edu