Thanks for the info. Diluted NaOH (5-10%) may work as well. ---------------------------------------------- You might try a 5% HCL dip for 30 seconds. Justin C. Borski MEMS Program Manager Advanced MicroSensors Inc. jborski at advancedmicrosensors.com www.advancedmicrosensors.com -----Original Message----- From: Allen Chou [mailto:chou_allen at yahoo.com] Sent: Wednesday, May 21, 2003 7:11 PM To: mems-talk at memsnet.org Subject: [mems-talk] etch of tungsten oxide Hi, Does any one know any chemical that can remove the oxidized surface tungsten film without appreciable damage on the tungsten? Thanks, Allen __________________________________ Do you Yahoo!? The New Yahoo! Search - Faster. Easier. Bingo. http://search.yahoo.com __________________________________ Do you Yahoo!? Yahoo! Calendar - Free online calendar with sync to Outlook(TM). http://calendar.yahoo.com