Ken,
Have you tried Lawrence Semiconductor Laboratories?
They're in Tempe, Arizona.
Phone # 602-438-2300
FAX # 602-438-9591
Regards,
Brent E. Burns, PhD
Manager
Integrated Micro Sensors Group
Northrop Grumman ESID
Hawthorne, CA
Brent_Burns@ccmail.northgrum.com
brentburns@earthlink.net
______________________________ Reply Separator _________________________________
Subject: Epi Etch stop layer Suppliers
Author: "Ken Westra" at INTERNET
Date: 9/15/97 11:17 PM
Hi,
I'm looking for suppliers of boron doped/Ge stress compensated epi
layers on 4" Si wafers. Any suggestions ?
Ken Westra
Ken Westra PhD
Staff Scientist
Alberta Microelectronic Centre
# 318 11315 87 Ave
Edmonton Alberta Canada
T6G 2T9
Phone: 403 492 5570 ext 234
Fax: 403 492 1643