Hi, Levent,
send a fax to Sico Meiningen Wafer GmbH (Germany)
++49-3693-71315
They buy used wafers and thin them down, so they're relatively cheap.


> Date:          Thu, 25 Sep 1997 12:00:23 -0400 (EDT)
> From:          lxy9@po.CWRU.Edu (Levent Yobas)
> Subject:       looking for vendors of 150 micron thick wafers
> Reply-to:      lxy9@po.CWRU.Edu (Levent Yobas)
> To:            MEMS@ISI.EDU

> Anyone knows about companies selling 150 micron
> thick (or shall I say 100-200 micron) silicon wafers
> at a reasonable price. I can buy a dozen or more
Mit freundlichen Gruessen, Kai Hiltmann

mailto:Kai.Hiltmann@IMIT.Uni-Stuttgart.de    http://www.IMIT.Uni-Stuttgart.de
K. Hiltmann
c.o. IMIT
W.-Schickard-Str. 10
D-78052 Villingen-Schwenningen

Tel. ++49-7721-943-236
Fax  ++49-7721-943-210


reply