David You can contact Applied Materials Inc (PVD Al-Plug Division) as they have done a lot of work in Process/Technology Development for 200mm & 300mm Ni-V technology. David Ovrokzkywrote: Hello everybody, Where can I find the recommended recipe for Ni/7%V target in MRC sputter. I have tried searching the web, but without successes. I appreciate any help. David Ovrutsky Process Engineer Chip Size Packaging _______________________________________________ MEMS-talk@memsnet.org mailing list: to unsubscribe or change your list options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk Hosted by the MEMS Exchange, providers of MEMS processing services. Visit us at http://www.memsnet.org/ (Pramod Gupta) 20800 Valley Green Dr., # 445 Cupertino, CA 95014 Phone: (408) 253-1646 --------------------------------- Do you Yahoo!? Yahoo! SiteBuilder - Free, easy-to-use web site design software