durusmail: mems-talk: Ni/7%V sputtering
Ni/7%V sputtering
Ni/7%V sputtering
TEL Klaus Beschorner
2003-08-10
> Where can I find the recommended recipe for Ni/7%V target in MRC sputter.
> I have tried searching the web, but without successes.

David,
any reason why you can not just ask your supplier ?
KDF makes the MRC batch machines now, and TFE is their european rep.

The recipe will definitely depend on the type of target you are using.

best regards,
klaus

--

                        (TEEL)          Tokyo Electron Europe Limited
                                        PVD Process Support  (ex MRC)
Klaus Beschorner                                   Tel +49-7033-45683
Drosselweg 6                                       Fax +49-7033-45631
71120 Grafenau, Germany                       Mobile +49-174 315 7754


reply