Anand,

A good reference for photolithography on three dimensional structures is:

N. Pham, T. Scholtes, R. Klerk, B. Wieder, P. Sarro, J. Burghartz, "Direct Spray
Coating of Photoresist for MEMS Applications," Proceedings of SPIE, vol. 4557,
2001, pp. 312-319

I am a process engineer specializing in the development of processes for use on
the spray coating system mentioned in this article, and so have quite a bit of
experience on a wide array of device designs, so if you have any further
questions, or need clarification on any topics mentioned in the above paper,
feel free to contact me at any time.

Best Regards,
Chad Brubaker

EV Group       invent * innovate * implement
Technology - Tel: (602) 437-9492, Fax: (602)437-9435 e-mail:
C.Brubaker@EVGroup.com, www.EVGroup.com

This message and any attachments contain confidential or privileged information,
which is intended for the named addressee(s) only. If you have received it in
error, please notify the sender immediately and then delete this e-mail. Please
note that unauthorized review, copying, disclosing, distributing or otherwise
making use of the information is strictly prohibited.


 -----Original Message-----
From:   mems work [mailto:mems_work@hotmail.com]
Sent:   Sunday, August 03, 2003 3:26 PM
To:     mems-talk@memsnet.org
Subject:        [mems-talk] Electrodes in Microchannel

Hi..
     Can anyone point to me to papers on making electrodes in a
microchannel for a microfluidic application with electrophoresis and
electroosmosis or MHD requirements...

Also any pointers to photoresist patterning of the bottom and sidewalls of a
silicon microchannel ?


Thanks,
Anand

_________________________________________________________________
MSN 8 helps eliminate e-mail viruses. Get 2 months FREE*.
http://join.msn.com/?page=features/virus


_______________________________________________
MEMS-talk@memsnet.org mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/


reply