Dear all, is there anyone, who has worked on structuring platinum with wet etchants? I have tried aqua-regia (3parts HCl, 1part HNO3) of 36 %, but could not remove any Pt from my wafers. I am using ordinary resist on top of the Pt for structuring. Any suggestions on aqua regia or other chemicals that could etch Pt are greatly appreciated. Regards, Michael ================================================== | Michael Koch | | University of Southampton | | Department of Electronics and Computer Science | | Southampton SO17 1BJ | | England | | | | Tel.: +44 (0)1703 593737 | | Fax.: +44 (0)1703 593029 | | email: M.Koch@soton.ac.uk | ==================================================