but i dont have PLD in my clean room just E-beam evaporator but the system is down i need to fabricate my wafer urgently so does electroless gold able to deposit gold onto my wafer???? --- Ganesh Kumarawrote: > You can try to deposite gold on SiO2 using Pulsed > Laser Deposition(PLD) > technique. PLD deposition of gold is the most > adhesive to SiO2 as per my > experience. > > > >From: Ah Gong > >Reply-To: General MEMS discussion > > >To: mems-talk@memsnet.org > >Subject: [mems-talk] How to deposit gold onto a > silicon dioxide or onto > >aluminium > >Date: Thu, 21 Aug 2003 09:01:49 +0800 (CST) > > > >Is it possible to deposit gold onto a silicon > dioxide > >or aluminium layer using bright electroless gold > >solution as i had been trying to do so but to no > avail > >maybe someone can recommend me the best way to > deposit > >gold onto the wafer to do MEM switches or better > using > >the elctroless gold solution which i had bought > > > >===== > > > > > >__________________________________________________ > >Do You Yahoo!? > >Stand a chance to win cash prizes! > >http://yahoo.com.sg/millionaire > > > >_______________________________________________ > >MEMS-talk@memsnet.org mailing list: to unsubscribe > or change your list > >options, visit > http://mail.mems-exchange.org/mailman/listinfo/mems-talk > >Hosted by the MEMS Exchange, providers of MEMS > processing services. > >Visit us at http://www.memsnet.org/ > > _________________________________________________________________ > Access Hotmail from your mobile now. > http://server1.msn.co.in/sp03/mobilesms/ Click here. > > > _______________________________________________ > MEMS-talk@memsnet.org mailing list: to unsubscribe > or change your list > options, visit > http://mail.mems-exchange.org/mailman/listinfo/mems-talk > Hosted by the MEMS Exchange, providers of MEMS > processing services. > Visit us at http://www.memsnet.org/ ===== __________________________________________________ Do You Yahoo!? Play now and stand a chance to win cash prizes! http://yahoo.com.sg/millionaire