Dear Ah, It is necessary first to deposit nickel onto your glass substrate. Bright Electroless Gold will deposit onto the nickel. Transene Company (www.transene.com) offers products suitable for nickel and gold plating. Or, feel free to contact me directly. Christopher Christuk Transene Company Tel: 978 777 7860 Email: Christopher@transene.com -----Original Message----- From: Ah Gong [mailto:police_post@yahoo.com] Sent: Sunday, August 24, 2003 6:10 AM To: General MEMS discussion Subject: Re: [mems-talk] How to deposit gold onto a silicon dioxide or ontoaluminium but i dont have PLD in my clean room just E-beam evaporator but the system is down i need to fabricate my wafer urgently so does electroless gold able to deposit gold onto my wafer???? --- Ganesh Kumarawrote: > You can try to deposite gold on SiO2 using Pulsed > Laser Deposition(PLD) > technique. PLD deposition of gold is the most > adhesive to SiO2 as per my > experience. > > > >From: Ah Gong > >Reply-To: General MEMS discussion > > >To: mems-talk@memsnet.org > >Subject: [mems-talk] How to deposit gold onto a > silicon dioxide or onto > >aluminium > >Date: Thu, 21 Aug 2003 09:01:49 +0800 (CST) > > > >Is it possible to deposit gold onto a silicon > dioxide > >or aluminium layer using bright electroless gold > >solution as i had been trying to do so but to no > avail > >maybe someone can recommend me the best way to > deposit > >gold onto the wafer to do MEM switches or better > using > >the elctroless gold solution which i had bought > > > >===== > > > > > >__________________________________________________ > >Do You Yahoo!? > >Stand a chance to win cash prizes! > >http://yahoo.com.sg/millionaire > > > >_______________________________________________ > >MEMS-talk@memsnet.org mailing list: to unsubscribe > or change your list > >options, visit > http://mail.mems-exchange.org/mailman/listinfo/mems-talk > >Hosted by the MEMS Exchange, providers of MEMS > processing services. > >Visit us at http://www.memsnet.org/ > > _________________________________________________________________ > Access Hotmail from your mobile now. > http://server1.msn.co.in/sp03/mobilesms/ Click here. > > > _______________________________________________ > MEMS-talk@memsnet.org mailing list: to unsubscribe > or change your list > options, visit > http://mail.mems-exchange.org/mailman/listinfo/mems-talk > Hosted by the MEMS Exchange, providers of MEMS > processing services. > Visit us at http://www.memsnet.org/ ===== __________________________________________________ Do You Yahoo!? Play now and stand a chance to win cash prizes! http://yahoo.com.sg/millionaire