Hello everyone , I am trying to find some suitable etchant for W and Cu .It should etch Cu and W but not BST(Barium strontium titanate) .Can anybody share his/ her experience in this regard. Also I am trying to do some lift off of 0.2 micron thick Cu(using negative PR) on BST/Alumina substrate. This process works well for BST/Si but not for BST/Alumina.( my alumina substrate is much rougher than Si wafer) how important does the surface roughness play a role in lift off process? Any answers / leads will be very much appreciated. Thanks Dipankar Ghosh OFFICE ADDRESS :- MATERIALS RESEARCH CENTER, ROOM 322 , RB-1, 1001 CAPABILITY DRIVE, CENTENNIAL CAMPUS, NCSU, RALEIGH , NC 27695-7919 USA PH- 919 515 5049 FAX- 919 515 3419 ____________________________________________________________ Get advanced SPAM filtering on Webmail or POP Mail ... Get Lycos Mail! http://login.mail.lycos.com/r/referral?aid=27005