durusmail: mems-talk: Ni diffusion on Au under 800C
Ni diffusion on Au under 800C
Ni diffusion on Au under 800C
FungWaHong@mrst.com.cn
2003-09-18
David

The content of P is about 6%. I can't increase the concentration because of
customer requirement. I did an experiment with  fresh solutions
(Electroless Ni, pretreatment solution, and Au plating solution) and it
seems to be no improvement.

Benny Hong