hi experts, i am member of this group and PG student in india. i am doing Ni electroplating first time. if anyone have any experience please suggest me which metal should sputter ( Cu, Au, Cr)for su-8 resis mold and which plating solution and condition would be best. thanks a lot. RAvindra Mukhiya M. Tech. Student India. Email: ravindramukhiya@rediffmail.com mukhiya04@yahoo.com. ___________________________________________________ Meet your old school or college friends from 1 Million + database... Click here to reunite www.batchmates.com/rediff.asp