How to etch gold ( 3 micron thick0
kris
2003-09-26
try in KI+I2+H2o

u will get that recipe by browsing

kris
--- gokul ramamani  wrote:
> Hi,
>
> Does anybody know any method by which i can etch 3
> micron meter thick gold??
>
> Gokul
>
>
_________________________________________________________________
> Calling all NRIs! Avail of the best financial
> services.
>
http://server1.msn.co.in/msnspecials/nriservices/index.asp
> Smile all the way
> with ICICI Bank.
>
>
> _______________________________________________
> MEMS-talk@memsnet.org mailing list: to unsubscribe
> or change your list
> options, visit
>
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS
> processing services.
> Visit us at http://www.memsnet.org/


__________________________________
Do you Yahoo!?
The New Yahoo! Shopping - with improved product search
http://shopping.yahoo.com

reply