Is it purple in color? If so you can remove it easily by wiping with hydrogen peroxide on occasion. Follow with a di water rinse then isopropal alcohol and then pump your system to an appropriate base pressure. Condition the chamber by running an etch cycle and you should be good to go. Bob Henderson