Dear George Steimle, I advise you to look through the paper: W.Lang et al. Absorbing layers for thermal infrared detectors, Sensors and Actuators A, vol. 34 (1992), pp.243-248. With best regards, Alexander G. Kozlov ----- Original Message ----- From: "George Syeimle"To: Sent: Wednesday, October 15, 2003 8:21 PM Subject: [mems-talk] Platinum Black > We are looking for a platinum black plating chemistry and process. We are having trouble finding a supplier or any information, > any help will be appreciated. > Thanks for any help, > George Steimle > _______________________________________________ > MEMS-talk@memsnet.org mailing list: to unsubscribe or change your list > options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk > Hosted by the MEMS Exchange, providers of MEMS processing services. > Visit us at http://www.memsnet.org/ > >