durusmail: mems-talk: Thin SU-8, SU-8 2002
Thin SU-8, SU-8 2002
2003-11-13
3" sapphire wafer
2003-11-13
2003-11-13
Gold etch without etching copper?
2003-11-14
Thin SU-8, SU-8 2002
Brubaker Chad
2003-11-13
Werner,

What kind of questions do you have?  We've got experience in both coating and
exposure many grades of SU-8 (both original and 2000) in many thicknesses,
including the a 2um film of SU-8 2002.  Did you have questions in mind regarding
a specific application?  Or are you looking for more general info?  Perhaps you
are experiencing a problem and are looking for some possible suggestions for the
problem.

Whatever the case may be, feel free to contact me (my information is below) with
your interest.


Best Regards,

Chad Brubaker

EV Group       invent * innovate * implement
Technology - Tel: (602) 437-9492, Fax: (602)437-9435 e-mail:
C.Brubaker@EVGroup.com, www.EVGroup.com

This message and any attachments contain confidential or privileged information,
which is intended for the named addressee(s) only. If you have received it in
error, please notify the sender immediately and then delete this e-mail. Please
note that unauthorized review, copying, disclosing, distributing or otherwise
making use of the information is strictly prohibited.


 -----Original Message-----
From:   mems-talk-bounces+c.brubaker=evgroup.com@memsnet.org [mailto:mems-talk-
bounces+c.brubaker=evgroup.com@memsnet.org]  On Behalf Of Werner Karl
Sent:   Thursday, November 13, 2003 9:33 AM
To:     mems-talk@memsnet.org
Subject:        [mems-talk] Thin SU-8, SU-8 2002

Dear All,

     I am looking for someone with experience using thin permanent layers of
SU-8 (< 2 um), specifically SU-8 2002? Best regards,

Werner.



_______________________________________________
MEMS-talk@memsnet.org mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/


reply