Hello,

Does anybody know if gold mask can be used for TMAH etching? I have 1000 A gold
layer (with 100 A Cr) on a Si wafer. I used 5% TMAH and etch for half an hour.
The result is much below the typical etch rate.

Before etching I removed native oxide with HF.

Thank you for your help

Martyna