Hi Jen, If you are dealing with small quantities of dice you can also try the method below using petri dishes and teflon tweezers. 1. PR stripper soak 2. Acetone soak 3. Methanol soak (optional) 4. DI water soak 5. Diluted HF soak 6. Di water soak For this to work, you have to watch out for cross contamination (use only a specific petri dish for each soak and clean everytime before use) Phil Tabada UC Davis PhD Candidate >From: Jen Robertson>Reply-To: General MEMS discussion >To: mems-talk@memsnet.org >Subject: [mems-talk] cleaning small chips >Date: Fri, 19 Dec 2003 17:04:59 -0800 (PST) > >Hi- > >Is there a good way to clean small (<5mm square) silicon chips? Our chips >have lots of visiable residues after the dicing process, either from the >dicing tapes or wafer dusts. We have tried soaking in many different >solvents but cannot seem to get rid of them. These chips have fragile MEMS >structures on them and will break if we use ultrasonic agitation. Any >suggestion would be greatly appreciated. Thanks! > > >Jen > > >--------------------------------- >Do you Yahoo!? >Free Pop-Up Blocker - Get it now >_______________________________________________ >MEMS-talk@memsnet.org mailing list: to unsubscribe or change your list >options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk >Hosted by the MEMS Exchange, providers of MEMS processing services. >Visit us at http://www.memsnet.org/ _________________________________________________________________ Make your home warm and cozy this winter with tips from MSN House & Home. http://special.msn.com/home/warmhome.armx