Hi all,
I've encountered some problem with resist deposition. UVIII (the
e-beam/deep-UV resist I use from Shipley) covers the holes I want to
coat (5µm diameter, 1µm depth) but does not penetrate it.
Does anybody know where this problem comes from?
Thanks for your suggestions.