Do not know about gold etchant but you can certainly etch Ni using Piranha (5H2So4+1H2O2). This is a self heating solution. Add H2O2 just before the reaction. Niv ----- Original Message ----- From: hare krishnaDate: Friday, January 16, 2004 1:01 pm Subject: [mems-talk] Etching Problem > Dear All, > > I am a student of M.Tech in IIT Kanpur and i am working in the > field of electronic materials. > I have to etch gold and nickel, but the microetchant should not > affect the negative photoresist (SC100).The film deposited is > Silicon (substrate) / Nickel / Gold / photoresist(during > pattering). I have used aquaregia (aquaregia:water :: 1:2 ) for 5 > min.,for the microetching of both nickel and gold but it stripped > away the photoresist only. > What should i do now. > > Thanking You > Your's Sincerely > Hare Krishna > > Yahoo! India Mobile: Ringtones, Wallpapers, Picture Messages and > more.Download now. > _______________________________________________ > MEMS-talk@memsnet.org mailing list: to unsubscribe or change your list > options, visit http://mail.mems-exchange.org/mailman/listinfo/mems- > talkHosted by the MEMS Exchange, providers of MEMS processing > services.Visit us at http://www.memsnet.org/ >