durusmail: mems-talk: Pt etching
Pt etching
1997-02-20
Pt etching
Rob
1997-02-20
Other than using lift off I would like to pattern Pt by ethcing.
Does anyone know where I could fine the etch rate of Pt using Aqua Regia
at 70 C (3 part hydrocloric 1 part Nitric acid)?

Thank you,

Rob
rob@casimir.eecs.uic.edu
Microfabrication Application Laboratories
University of Illinois at Chicago


reply