Try 1165 or pure NMP heated to 80 C Greg -----Original Message----- From: Hunter, Luke L [mailto:llhunte@sandia.gov] Sent: Monday, February 02, 2004 1:45 PM To: 'mems-talk@memsnet.org' Subject: [mems-talk] Quickly dissolving thick PMMA MEMS folk, I know that acetone works for dissolving PMMA but is there something that will work much faster, maybe 10 times? PMMA thickness is between 300 microns and 1500 microns. Currently it takes 3 days to dissolve 1500 micron thick PMMA in acetone. Thanks _______________________________________________ MEMS-talk@memsnet.org mailing list: to unsubscribe or change your list options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk Hosted by the MEMS Exchange, providers of MEMS processing services. Visit us at http://www.memsnet.org/