Thermal evaporation might workout for your application and we offer foundry services for this kind of deposition. You can check our web site at www. triontech.com and click on foundry page.. If you really need to do low temperature films like you describe I would contact a company named Jet Process located in New Haven,CT phone: 203-777-6000. Bob Henderson