hello,all,
I am trying to cure MAA in a PDMS female mold, but the PMAA can not be peeled
off from the PDMS
mold.the reason might be the diffusion of MAA into the PDMS mold or adhesion
(bonding) of MAA to PDMS.
Id like your opinion to solve this problem with PDMS or recommend me another
kind of rubber instead
of PDMS.
your responsed would be greatly appreciated!
Chunmeng Lu
Department of Chemical Engineering