Miguel (and everyone else asking etching questions)-- Do a literature search on etchants for micromachining. You will find this paper: http://microlab.berkeley.edu/labmanual/chap1/JMEMSEtchRates2(2003).pdf 5:1 BHF etches SiO2, but not Nb or Si. There are other etchant/material combinations that provide reasonable selectivity. --Kirt Williams ----- Original Message ----- From:To: Sent: Sunday, May 23, 2004 12:15 AM Subject: [mems-talk] Niobium resistant Silicon Etching > Hello Mems-Talkers, > > Does anybody know of a wet etchant or dry etchant which will selectively > etch Silicon and or SiO2 while leaving the Niobium unetched? Alternately I may > grow the Niobium on SiO2 layer as opposed to the Silicon and use the SiO2 as an > etch stop. After I will need to etch the SiO2 from under the Niobium. Keep up > the good work everybody.Thank You. > > Sincerely, > > Miguel Zorn > _______________________________________________ > MEMS-talk@memsnet.org mailing list: to unsubscribe or change your list > options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk > Hosted by the MEMS Exchange, providers of MEMS processing services. > Visit us at http://www.memsnet.org/