> We need suggestion from you about Ti and TiN process. Hi , it would pobably help your cause to tell us which machine you use. Depending on the setup and post-processing, single chamber Ti/TiN is possible, and used in the CMOS semicunductor industry. best regards, klaus Klaus Beschorner Metron Technology Europe, PVD (Eclipse) Process Manager