Si surface roughness in DRIE process
Sunny Kedia
2004-05-28
Qing Yao,

An EPW etch ( Ethylenediamine pyrocatechol and water) can be done to improve
the surface roughness, There is a paper "Anisotropic Si Etching Technique
for optically smooth surfaces" by Sasaki Metal in Eurosensors xv.

Sunny Kedia



reply