Hi, The total answer is image reversal. I will send you a more complete email shortly. Bill Moffat -----Original Message----- From: tao liu [mailto:liutao@gmail.com] Sent: Thursday, May 27, 2004 3:10 PM To: mems-talk@memsnet.org Subject: [mems-talk] About laser holography Hi, I use HeCd laser to do holography with two-beam interference. The wavelength is 446nm. My sample is PR1805/SiO2/GaAs. The period is 1.5um. The sample is exposed twice to form a crossed grating. After exposure and development, I can always see the non-uniformity on the sample surface: some area has good exposure, some area has under-exposure, and some area has over-exposure. Because the time for a single exposure is only ~ 3s and the development is also only ~ 3s, I suspect that this is caused by the very short development time. (I cannot use long development time for my present conditions. Otherwise all the patterns will be lost.) Can anybody give me some hints for that? Thanks. Best regards, Tao _______________________________________________ MEMS-talk@memsnet.org mailing list: to unsubscribe or change your list options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk Hosted by the MEMS Exchange, providers of MEMS processing services. Visit us at http://www.memsnet.org/