hello
I am trying to find the etchant of TaAl. Now I use lift-off method to
pattern the TaAl.
It's a diifficult job and has cleaning problems.
I am very glad if you recommend the etchant of TaAl.
E-mail : smallest@secns.sec.samsung.co.kr
Domestic
Tel : 0331-200-8748
011-289-1598
Fax : 0331-200-3307
Foreign
Dong-Sik Shim
SAMSUNG ELECTRONIC CO., LTD
416,Maetan-3Dong, Paldal-Gu,
Suwon city, Kyungki-Do, Korea 442-742
Tel :82-331-200-8748
Fax :82-331-200-3307
[Moderator's note: I excised four lines after "Domestic", above,
because they contained non-ASCII characters that were incompatible
with the Content-type: of the message as I received it, and which
caused some difficulty with my mail reader. CMR]