Hi Jon,

do you know how if there are any restrictions of FIB cutting regrding the
thickness of the cutted material?

Thanks

J.


> Josef,
> If classical sawing creates a problem you can use a dual beam FIB to
create
> the cross-section.  If you don't have access to such a tool you could try
> scribing the back side and the cleaving it.
> Jon Hiller