durusmail: mems-talk: Etching Tantalum-Rhenium and Rhenium
Etching Tantalum-Rhenium and Rhenium
2004-06-14
Etching Tantalum-Rhenium and Rhenium
chong hanwoo
2004-06-14
Hi,

Does anyone has experience on wet etching Tantalum-Rhenium (Ta-Re) thin film
formed by means of co-sputtering of Ta and Re?

Also, is there any convenient way to wet etch Re or Ta-Re without damaging
Tungsten Carbide?

thanks

Han